INFLUENCE OF HEAT TREATMENT ON PROPERTIES OF EN AW 6082 ALUMINIUM ALLOY
DOI:
https://doi.org/10.12776/ams.v21i1.553Keywords:
severe plastic deformation, tension test, aluminium alloys, wearAbstract
The main aim of this work is to point out on possibility of properties improving of the aluminium alloy EN AW 6082 (AlSi1MgMn) with an appropriate combination of pre-ECAP solution annealing, the application of the severe plastic deformation by ECAP technology (equal channel angular pressing) and post-ECAP artificial aging. The effect of the severe plastic deformation and artificial aging on the alloy structure was evaluated by metallographic analysis, and alloy mechanical properties by uniaxial tensile test at room temperature, the Vickers hardness and by tribology test of resistance to abrasive wear. As a result of strain hardening by severe plastic deformation it reaches the improvement in hardness (by 56%), strength characteristics (yield strength by 92%, tensile strength by 29%) and abrasion wear resistance is 28 %.