QUANTIFICATION OF CORROSION ACTIVITY ON HDG STEEL SHEETS DURING CYCLIC DIP TESTS IN CLASSICAL AND ECOLOGICAL SALT SOLUTIONS

Authors

  • Maroš Halama
  • Ying Zhu
  • Karol Kovaľ
  • Janette Brezinová

DOI:

https://doi.org/10.12776/ams.v20i1.242%20p-

Keywords:

corrosion monitoring, electrochemical noise, activity, zinc surface

Abstract

The paper is focused on the part of complex work dealing with verification of functionality of non-destructive technique of electrochemical noise applied on HDG steel sheets samples with different surface treatment, namely on samples to be treat with Cr3+, anticorrosion oil and non-oiled and non-passivated ones. Besides monitoring of quality of surface treated zinc sheets (activity/passivity) by ENA technique an extension of corrosion deterioration was quantified gravimetrically after 3, 15, 22 and 30 days of exposure in 3 % NaCl, 3% ecological salt mainly composed of MgCl2, CaCl2 and condensation chamber. Corrosion products were observed with support of SEM microscopy with EDX analysis.

Downloads

Published

2014-03-31

How to Cite

Halama, M. ., Zhu, Y. ., Kovaľ, K. ., & Brezinová, J. . (2014). QUANTIFICATION OF CORROSION ACTIVITY ON HDG STEEL SHEETS DURING CYCLIC DIP TESTS IN CLASSICAL AND ECOLOGICAL SALT SOLUTIONS. Acta Metallurgica Slovaca, 20(1), 86–96. https://doi.org/10.12776/ams.v20i1.242 p-